Getting FED UP with KOH yet??
Howdy Folks: this hho experimenter has been running KOH for maybe a month now and I'm still getting the dang brown bloom that I had with NaOH. I can drain off to a degree, but I don't like it at all for show and tell...
and when time comes for cleaning my neutral plates, it will be a pain. I've used vinegar... anybody out there using citric acid, or maybe potassium citrate??
The brown GOOO is everywhere!
Hi guys! I just signed on.......
I too am looking for an answer to the brown GOOO. I've built 7 different generators over the last year. I started with wet cells, then brick, then dry cells. I made one dry cell where I used the 304ss cover plates. (16 plates. They had 304 printed on the back side. ) My latest one is a 16 plate, 6 X 6 dry cell. I've used Baking soda, lye, KOH...... I even put in a cooling coil just before the water entered the generator. No matter what I run or how I run it, as soon as it worms up (85-90 Deg. F) the brown goop starts to slowly show up. I've used tap, condensate, distilled. Distilled takes longer but the brown snow eventually forms. I'm starting to think its a voltage thing. What do you say????