hmm, speaking of glass wrap.
a person could fiberglass his setup after finding the optimum design.;)
Printable View
hmm, speaking of glass wrap.
a person could fiberglass his setup after finding the optimum design.;)
lol im a bit lost, what are we wrapping here?
because im thinking the whole plastic canister part, w/e its called
u want to wrap the stainless steel CELL that makes the HHO
here's a pic of what the current does if u do not wrap a cell
That is why u want to wrap with something like liquid electrical tape, or something that blocks current.
http://www.free-energy-info.co.uk/Ch10/Fig20.gif
thankyou very much!! saved me some time i would have wasted in the future lol
thats why I am thinking that dry is the way to go.
we should be able to come up with a rough lpm to Sq Inch value.
What about :
-+-S/S wool-+-S/S wool-+-
Use 316L flat plate for positive and perforated plate sandwiched with stainless steel wool for negative
ok have tried
1 = -+ works ok but over 160 Degrees at 21 amps - get about 0.7 LPM
2 = -N+ works near same as one
3 = -NN+ and 20 amp - 120 Deg and 1.4 LPM === at 28A - 1.8 LPM
4 = -NNNNN++NNNNN- 30A - 0.8 LPM
What happened to #4??????? why so low production??
next i want to try #4 split into -NNNNN+ to see what happens.