Originally Posted by
Philldpapill
I don't think my description was very clear. This gasket material will be compressed between plates. It's not just gooped in there and dried. As for the chemical stability, so far it looks good.... A cured sample has been sitting in a jar of KOH for over a week now, on a heat pad(>150°F). I suspect these are similiar conditions that it would face in an HHO cell. It cures fairly hard, so I think I could put a good bit of compression on it when I tighten down the cell.
And yes, hhonewbie, I've thought about "cooking" it in the oven for a while. The stuff SAYS it should set up in 3 hours in the open air, but of course that's BS. I'm going to let this stuff fully cure for 2 weeks before I pop it out of the mold.
It seems you have a heating pad, that's a good way to cure is quicker.
Good luck, i look forward to hearing more!