For those of you who blast your own plates, do you have a choice of material that has worked well for you and do you have any tips to share regarding blasting plate surfaces? I'm looking at starting with a 80-90 grit and then going with a 320 or so grit to finish them.


I found some shops locally to do my plates but after receiving their quotes I could have completed my cell in nickel 200 for the same price that they wanted just to media blast them.

What media have you used?